Insights / Design Guide

LSR Injection Molding Design Guide: Tolerances, Wall Thickness & Parting Lines

Direct answer

For LSR, specify ±0.05 mm on critical sealing features and ±0.10–0.25 mm on general dimensions, keep walls typically between 0.8 and 3.0 mm, and place parting lines away from sealing surfaces. Consistent draft, radiused transitions and early DFM review matter more than tightening every tolerance on the drawing.

Liquid silicone rubber is not a rigid material with a single shrink rate. It is a low-viscosity, platinum-cured elastomer that flows into fine detail, cures in seconds and then deflects under the smallest measurement force. That changes how a drawing should be dimensioned — and it is why copy-pasting a CNC tolerance block onto an LSR part usually creates cost without creating function.

1. Set tolerances by feature, not by habit

The most useful DFM conversation is not “what tolerance can you hold?” but “which features actually need to be controlled?” A sealing lip, a connector bore and a cosmetic cover have different functions, different measurement methods and very different cost sensitivity.

Practical starting tolerances for LSR parts. Confirm against part size, material hardness and the agreed inspection method.
Feature classTypical drawing toleranceWhat drives the result
General, non-sealing dimensions±0.10–0.25 mmPart size, shrinkage, cavity balance and free-state measurement.
Critical sealing diameters / bores±0.05 mmDatum scheme, low-force 2D vision measurement (video microscope), tool correction.
Wall thickness±10% or ±0.10 mmFlow length and cavity pressure; avoid combining a thin wall with a tight band.
Hole and slot position±0.05 mmPin location, gate position and material flow around the feature.
Flash at a sealing face0.02–0.05 mm maxParting-line design, venting and tool shut-off; specify with a boundary sample.
Flatness / coplanarity0.10 mmFixtured measurement at a defined temperature, not free-state on a bench.

Two rules make these numbers usable. First, define the datum and the gauge before approving the drawing; a soft part measured with a hard contact probe at unknown force will produce arguments, not data. Second, keep tight tolerances on as few features as possible. Every additional tight feature adds tool correction time, inspection time and scrap risk.

2. Wall thickness: design for flow and demolding

Most LSR parts work best with walls between about 0.8 and 3.0 mm. Below 0.8 mm, the material must fill a long, thin section before it cures; that demands higher injection pressure, precise venting and a carefully balanced runner. Above roughly 3–4 mm, cure time grows and thick-to-thin transitions become a source of distortion and compression-set variation.

  • Transition gradually. Use a taper of about 1:3 rather than an abrupt step. Sharp thickness changes create flow hesitation and stress.
  • Radius internal corners. A minimum internal radius of 0.25–0.5 mm reduces tearing during demolding and improves fatigue life at a sealing lip.
  • Design ribs thinner than the wall. A rib at 0.6–0.8× the nominal wall adds stiffness without creating a heavy curing section.
  • Core out thick sections. If a block of material is not functional, remove it. Thick silicone is expensive to cure and harder to control.

Thin walls and tight tolerances are not automatically compatible. If a 0.5 mm wall also carries a ±0.05 mm tolerance, expect tool iteration and a slower process window. Decide which requirement is functional before the tool is designed.

3. Parting lines: put them where they do no harm

A parting line is a controlled witness mark, not a defect to be hidden later. Place it away from sealing surfaces, sliding interfaces and cosmetic A-surfaces. On a valve seat or a connector bore, a parting line across the sealing path can create a leak path that no amount of post-trim will fix.

  • Vent at the last point to fill. Trapped air causes short shots and burns; venting should be part of the parting-line layout, not an afterthought.
  • Draw the line on the drawing. Show the intended parting-line location and the allowed witness mark. Ambiguity becomes a dispute at first article.
  • Prefer tear-trim-friendly geometry. Where secondary or tear trimming is required, keep a clean, accessible edge path. A cold runner reduces flash but does not remove the need for trim access.
  • Add draft early. Typically 0.5–2° of draft on vertical walls — toward the upper end on deep walls and 60–80 Shore A grades — makes demolding predictable and protects the surface finish.

4. The DFM checklist we use before tooling

  • Critical features identified, with datum and inspection method agreed.
  • Wall thickness map reviewed; thin and thick regions flagged.
  • Parting line and gate location drawn on the model.
  • Draft, radii and undercut strategy confirmed.
  • Flash allowance and cosmetic boundary samples defined.
  • Material hardness and compliance route matched to the application.
  • Overmold substrate, if any, reviewed for bond and thermal expansion.

None of this replaces a first-article inspection. It simply moves the expensive corrections from steel to screen. If you have a drawing to review, send the CAD and the functional requirements — a second set of eyes is most useful when we know what the part must do, not only what it looks like.