Toolroom
Mold Design Review
Runner, gating and parting-line review before any steel is cut.
Capabilities · LSR & Multi-Shot
Injection molding, overmolding, multi-shot 2K and prototyping under one roof — so tolerance, bonding and flash control stay consistent from sample to mass production.
01 / Cold-runner, flash-controlled molding.
Liquid silicone rubber is metered as a two-part liquid, injected into a heated mold and cured in seconds. The tool, the cold runner and the venting strategy decide whether that speed becomes repeatable precision.
We design the runner balance, gate location and venting around the part geometry, then lock the process window during sampling. The result is stable cavity-to-cavity dimensions, minimal flash and less post-trim handling — the cost drivers that usually hide in a piece price.
02 / Bonding soft silicone to rigid substrates.
Overmolding replaces gaskets, adhesives and secondary assembly with a single, sealed component. The engineering work is in substrate selection, surface preparation and cure control.
We mold LSR directly onto PC, PA, PBT and prepared metal inserts. Adhesion can be chemical (primer-assisted), mechanical (undercuts, through-holes, textured surfaces), or primer-free using self-adhesive LSR grades and plasma surface treatment — the preferred routes for medical and Infant & Mom care programs where chemical primers are restricted. Each route is validated with pull or peel testing before release.
Insert molding places a pre-formed insert into the mold and encapsulates it with plastic or silicone. Overmolding molds a second material over an existing substrate, often to add grip, sealing or chemical resistance. In practice, insert molding is a subset of overmolding: the insert is the substrate, and the LSR is the overmolded layer.
| Substrate | Adhesion route | Process note |
|---|---|---|
| PC | Primer-assisted chemical bond | Pre-dry; control mold temperature (HDT limit) and select PC-safe primers to prevent environmental stress cracking (ESC) or warpage. |
| PA6 / PA66 | Primer or mechanical interlock | Moisture-sensitive; pre-dry and validate bond after conditioning. |
| PBT | Primer-assisted | Good dimensional stability; verify primer compatibility per grade. |
| Aluminum | Conversion coating + primer | Degrease, anodize or conversion-coat, and mask unbonded zones before priming. |
| Stainless steel | Primer or mechanical lock | Surface finish and cleanliness drive repeatability. |
| Brass | Primer + mechanical feature | Ultrasonic clean to remove machining oils; watch amine or sulfur contamination from machining fluids. |
Substrate grade, surface energy and primer selection must be confirmed with sample bonding and pull testing for each project. For medical and Infant & Mom care programs, primer-free routes — self-adhesive LSR grades or plasma activation — are available on PC, PA and PBT.
03 / Automated 2K molding for high-volume integrity.
When manual insert handling introduces alignment variation or contamination risks, multi-shot injection integrates rigid thermoplastics and LSR inside a single automated cycle — delivering tight sealing and repeatable assembly geometry.
Using rotary or index-plate tooling, the freshly molded substrate transfers directly into the silicone cavity while still warm and pristine, creating strong chemical adhesion and lowering unit labor cost at scale.
04 / Proof before volume tooling
A bridge tool is a controlled way to buy production data early. We use pilot-cavity tooling to validate material, shrinkage, parting lines and assembly fit.
Tooling accuracy starts with the steel. Cavity dimensions, parting-line alignment, ejection and thermal layout are reviewed in the same engineering cycle as the part itself.
Inside the toolroom
Short clips from our own toolroom — design review, CNC cavity machining, die-sinking and mold maintenance.
Toolroom
Runner, gating and parting-line review before any steel is cut.
Toolroom
Cavity and core plates machined to the tool drawing.
Toolroom
Fine detail and sharp shut-offs burned after milling.
Toolroom
Wear inspection, polishing and repair between production runs.
Material & process comparison
The two silicone families behave differently in tooling, cycle time and dimensional control. Choose the process that matches the part, not the material name alone.
| Criterion | LSR (Liquid Silicone Rubber) | Solid Silicone (HCR) |
|---|---|---|
| Material form | Two-part low-viscosity liquid, pumped and metered | High-consistency gum, catalyst added and worked as a solid |
| Viscosity / flow | Low viscosity; fills thin walls, fine detail and long flow paths | High viscosity; limited flow, requires compression or transfer molding |
| Cure chemistry | Platinum-catalyzed addition cure; fast and controllable | Peroxide or platinum cure; longer, less automated cycles |
| Molding method | Injection molding with a cold runner | Compression molding or transfer molding |
| Typical cycle | Seconds to low minutes; highly automated | Minutes to tens of minutes; more manual handling |
| Flash & finishing | Minimal flash with cold-runner tooling; less deflashing | More flash and post-trim, especially on complex geometry |
| Tolerance & consistency | Repeatable dimensions; ±0.05 mm achievable on critical features | Good, but greater variation from loading, compression and trimming |
| Overmolding | Excellent bonding to plastics and metals with primer and process control | Limited; usually molded as a separate part and assembled |
| Automation & volume | High cavitation, low labor per part, suited to series production | Labor-intensive; better for large parts or lower volumes |
| Best fit | Precision seals, valves, connectors, thin-wall and high-volume parts | Large parts, thick sections, simple geometry and low-volume runs |
Tolerance figures are application-dependent. Critical dimensions should be identified on the drawing and reviewed during DFM; the final capability is confirmed by first-article inspection.
Material reference
Reference ranges for common liquid silicone rubber grades. Final values must come from the supplier datasheet for the exact grade and color used in your program.
| Property | Typical range | Reference / test | Engineering note |
|---|---|---|---|
| Hardness | 10–80 Shore A | ISO 48-4 / ASTM D2240 | Softer grades seal at lower force but demold and trim with more care. |
| Tensile strength | 4–10 MPa | ISO 37 | Formulation and filler loading dependent. |
| Elongation at break | 100–600% | ISO 37 | High elongation helps assembly and strain relief. |
| Tear strength | 10–40 kN/m | ASTM D624 | Critical for thin sealing lips and sharp edges. |
| Compression set | 15–35% | ISO 815 (22 h at 175 °C) | Lower set is preferred for static seals under sustained load. |
| Density | 1.10–1.25 g/cm³ | ISO 1183 | Varies with filler and pigment loading. |
| Service temperature | −60 to +200 °C; short peaks to 230 °C | Supplier datasheet | Confirm continuous rating for your grade and duty cycle. |
| Dielectric strength | 20–30 kV/mm | ASTM D149 | Relevant to insulating and high-voltage parts. |
| Biocompatibility | USP Class VI; ISO 10993-5 / -10 | Selected grades | Request test reports for the exact lot and formulation. |
| Food contact | FDA 21 CFR 177.2600; LFGB | Selected grades | Migration and sensory testing may be required by market. |
| Flame retardancy | UL94 V-0 | Selected grades | Verify with supplier; not all colors achieve the same rating. |
| Appearance | Translucent to opaque, pigmented | Visual / supplier | Pigments and additives can affect cure and compression set. |
Compliance is material- and market-specific. HY supplies material certificates, lot traceability and dimensional reports; regulatory sign-off remains with the device or product owner.
Next step
Send STEP/IGES plus your tolerance and compliance targets. We reply within 48 hours with a feasibility review, tooling approach and quotation. A full DFM report is provided after PO confirmation.